AN IMPROVEMENT IN A METHOD OF OBTAINING SINTERED BERYLLIUM OXIDE

Patent ·
OSTI ID:4157879

A process is presented which produces sintered BeO by calcining Be(OH)/ sub 2/ and sintering at 1700 deg C and high pressures. A small quantity of acid ions or Be salt of mineral acid is added up to 1%. BeSO/sub 4/ is recommended. This addition lowers the time, temperature, and pressure of sintering. (T.R.H.)

Research Organization:
Originating Research Org. not identified
NSA Number:
NSA-14-015053
OSTI ID:
4157879
Report Number(s):
GB 833667
Country of Publication:
United Kingdom
Language:
English

Similar Records

PREPARATION OF SINTERED BERYLLIUM OXIDE
Patent · Mon Oct 30 23:00:00 EST 1961 · OSTI ID:4029132

METHODS OF OBTAINING SINTERED BERYLLIUM OXIDE
Patent · Mon Oct 01 00:00:00 EDT 1962 · OSTI ID:4774699

IMPROVEMENTS IN METHODS OF PREPARING SINTERED BERYLLIUM OXIDE PRODUCTS
Patent · Tue Dec 12 23:00:00 EST 1961 · OSTI ID:4826259