Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

PREPARATION OF SINTERED BERYLLIUM OXIDE (in French)

Patent ·
OSTI ID:4029132
The raw material is Be(OH)/sub 2/ with a high proportion of the beta variety. A mineral acid (or a corresponding Be salt) is added in order to obtain only BeO. To prepare compacts, powdered BeO is sintered in a graphite mold at 1300 to 1500 deg C under a pressure of 2100 psi, after having been mixed with a neutron-absorbing substance such as B/sub 4/C. (EURATOM)
Research Organization:
Originating Research Org. not identified
NSA Number:
NSA-15-015989
OSTI ID:
4029132
Report Number(s):
BE 569700
Country of Publication:
Belgium
Language:
French

Similar Records

AN IMPROVEMENT IN A METHOD OF OBTAINING SINTERED BERYLLIUM OXIDE
Patent · Wed Apr 27 00:00:00 EDT 1960 · OSTI ID:4157879

SINTERING BEHAVIOR OF BERYLLIUM OXIDE
Journal Article · Thu Jun 01 00:00:00 EDT 1961 · Journal of the American Ceramic Society (U.S.) · OSTI ID:4065148

INVESTIGATION OF SINTERABLE POWDERS AND BERYLLIUM OXIDE PROPERTIES. Quarterly Report No. 4
Technical Report · Thu Apr 14 23:00:00 EST 1960 · OSTI ID:4140079