Alternate immersion stress corrosion testing of 5083 aluminum

Technical Report ·
DOI:https://doi.org/10.2172/6551622· OSTI ID:6551622

The stress corrosion susceptibility of Type 5083 aluminum--magnesium alloy in plate form and press-formed shapes was determined in the short transverse direction. C-ring type specimens were exposed to alternate immersion in a sodium chloride solution. The test equipment and procedure, with several innovative features, are described in detail. Statistical test results are listed for seven thermomechanical conditions. A certain processing scheme was shown to yield a work-strengthened part that is not sensitized with respect to stress corrosion cracking.