"SECONDARY" RECRYSTALLIZATION AND "TERTIARY" RECRYSTALLIZATION OF SOFT IRON COLD WORKED BY ROLLING AND ANNEALED UNDER HYDROGEN (in French)
Journal Article
·
· Compt. rend.
OSTI ID:4271745
Soft iron rolled and annealed under hydrogen presents a "secondary'' texture marked by the absence of (100) crystals parallel to the plane of the sheet. This texture formed of (110), (111), and (112) grains is, in general, replaced by a ''tertiary'' texture with large (110) STA001! grains. (tr-auth)
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-13-010069
- OSTI ID:
- 4271745
- Journal Information:
- Compt. rend., Journal Name: Compt. rend. Vol. Vol: 248
- Country of Publication:
- Country unknown/Code not available
- Language:
- French
Similar Records
TEXTURE DEFORMATION AND RECRYSTALLIZATION OF Fe-Ni (48% Ni) IN COLD ROLLING
(110) [001] Secondary Recrystallization Texture in Three Percent Silicon-Iron
Recovery and recrystallization in rolled tantalum single crystals
Journal Article
·
Sat Oct 31 23:00:00 EST 1959
· Fiz. Metal. i Metalloved.
·
OSTI ID:4171308
(110) [001] Secondary Recrystallization Texture in Three Percent Silicon-Iron
Journal Article
·
Fri Feb 28 23:00:00 EST 1958
· Journal of Applied Physics
·
OSTI ID:4344919
Recovery and recrystallization in rolled tantalum single crystals
Journal Article
·
Wed Aug 01 00:00:00 EDT 1979
· Metall. Trans., A; (United States)
·
OSTI ID:6062063