DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period August 31, 1960 thru September 30, 1960
Technical Report
·
OSTI ID:4019982
Two molybdenum ingots were produced, but both were contaminated during arc melting with water oxidation. Even though oxidized, both contained high residual carbon contents. The sllicon content of as-produced molybdenum powder decreased. All components of the purification train appeared to be functioning well. (auth)
- Research Organization:
- Oregon Metallurgical Corp., Albany
- NSA Number:
- NSA-15-025175
- OSTI ID:
- 4019982
- Report Number(s):
- NP-9559
- Country of Publication:
- Country unknown/Code not available
- Language:
- English
Similar Records
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period September 30, 1960 thru October 31, 1960
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period October 31, 1960 thur November 30, 1960
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period July 31, 1960-August 31, 1960
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4020702
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period October 31, 1960 thur November 30, 1960
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4019714
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period July 31, 1960-August 31, 1960
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4124019