DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period October 31, 1960 thur November 30, 1960
Technical Report
·
OSTI ID:4019714
The first low-oxygen, low-carbon, low-nitrogen arc-cast ingot was produced. The casting weighed 32 lb, was 3 3/4 in. high and 5 3/4 in. in diameter. No physical testing was begun on the material. A hydrogen gas sample was analyzed and was high in carbon monoxide and nitrogen content. A description of the entire molybdenum facility with photographs is presented. (auth)
- Research Organization:
- Oregon Metallurgical Corp., Albany
- NSA Number:
- NSA-15-025177
- OSTI ID:
- 4019714
- Report Number(s):
- NP-9561
- Country of Publication:
- United States
- Language:
- English
Similar Records
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period September 30, 1960 thru October 31, 1960
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period March 31--April 30, 1961
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period August 31, 1960 thru September 30, 1960
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4020702
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period March 31--April 30, 1961
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4039779
DEVELOP PROCESS FOR AND ARC CAST 25 TO 50 POUND INGOTS OF TIN REDUCED MOLYBDENUM. Progress Report for the Period August 31, 1960 thru September 30, 1960
Technical Report
·
Mon Oct 30 23:00:00 EST 1961
·
OSTI ID:4019982