Title: Process for strengthening aluminum based ceramics and material

Patent Application ·
OSTI ID:757162

A process for strengthening aluminum based ceramics is provided. A gaseous atmosphere consisting essentially of silicon monoxide gas is formed by exposing a source of silicon to an atmosphere consisting essentially of hydrogen and a sufficient amount of water vapor. The aluminum based ceramic is exposed to the gaseous silicon monoxide atmosphere for a period of time and at a temperature sufficient to produce a continuous, stable silicon-containing film on the surface of the aluminum based ceramic that increases the strength of the ceramic.

Research Organization:
Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
Sponsoring Organization:
US Department of Energy (US)
DOE Contract Number:
AC05-96OR22464
Assignee:
DOEGC; EDB-00:057978
Patent Number(s):
PATENTS-US-A9050371
Application Number:
9-050,371; TRN: AH200022%%69
OSTI ID:
757162
Resource Relation:
Patent File Date: 1998 Mar 31; Other Information: PBD: 1 Dec 1998
Country of Publication:
United States
Language:
English