Title: Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling

Authors:
; ; ;
Publication Date:
Sponsoring Org.:
USDOE
OSTI Identifier:
1359433
Grant/Contract Number:  
FG02-07ER46453; FG02-07ER46471
Resource Type:
Publisher's Accepted Manuscript
Journal Name:
Journal of Nuclear Materials
Additional Journal Information:
Journal Name: Journal of Nuclear Materials Journal Volume: 479 Journal Issue: C; Journal ID: ISSN 0022-3115
Publisher:
Elsevier
Country of Publication:
Netherlands
Language:
English

Citation Formats

Elbakhshwan, Mohamed S., Miao, Yinbin, Stubbins, James F., and Heuser, Brent J. Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling. Netherlands: N. p., 2016. Web. doi:10.1016/j.jnucmat.2016.07.047.
Elbakhshwan, Mohamed S., Miao, Yinbin, Stubbins, James F., & Heuser, Brent J. Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling. Netherlands. doi:10.1016/j.jnucmat.2016.07.047.
Elbakhshwan, Mohamed S., Miao, Yinbin, Stubbins, James F., and Heuser, Brent J. Sat . "Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling". Netherlands. doi:10.1016/j.jnucmat.2016.07.047.
@article{osti_1359433,
title = {Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling},
author = {Elbakhshwan, Mohamed S. and Miao, Yinbin and Stubbins, James F. and Heuser, Brent J.},
abstractNote = {},
doi = {10.1016/j.jnucmat.2016.07.047},
journal = {Journal of Nuclear Materials},
number = C,
volume = 479,
place = {Netherlands},
year = {2016},
month = {10}
}

Journal Article:
Free Publicly Available Full Text
Publisher's Version of Record
DOI: 10.1016/j.jnucmat.2016.07.047

Citation Metrics:
Cited by: 2 works
Citation information provided by
Web of Science

Save / Share: