Optical glass fabrication technology. 2: Relationship between surface roughness and subsurface damage

Journal Article · · Appl. Opt.; (United States)
DOI:https://doi.org/10.1364/AO.26.004677· OSTI ID:6046576

For glass grinding conditions where fracture is the principal mechanism, a constancy is found between the depths of surface roughness and subsurface damage. For a range of experimental conditions we find the ratio of subsurface damage to surface roughness to be 6.2--6.4 for bound diamond abrasive grinding. This is larger than the value reported for loose abrasive grinding (3.7--4.0). The constancy of this value has great practical importance. From a measurement of the surface roughness one can obtain an accurate estimate of the damage layer thickness that must be eliminated by polishing or subsequent grinding operations.

Research Organization:
Lawrence Livermore National Laboratory, Materials Fabrication Division, P.O. Box 808, Livermore, California 94550
DOE Contract Number:
W-7405-ENG-48
OSTI ID:
6046576
Journal Information:
Appl. Opt.; (United States), Journal Name: Appl. Opt.; (United States) Vol. 26:21; ISSN APOPA
Country of Publication:
United States
Language:
English