High-temperature oxidation of pure titanium in CO{sub 2} and Ar-10%CO{sub 2} atmospheres

Journal Article · · Oxidation of Metals
DOI:https://doi.org/10.1007/BF01670504· OSTI ID:563590
;  [1];  [2];  [3]
  1. Toyama Univ. (Japan)
  2. UCOM Co., Ltd., Akai (Japan)
  3. Tateyama Aluminum Industry Co., Ltd., Hayakawa (Japan)
The oxidation behavior of pure titanium has been investigated in the temperature range of 1000 K to 1300 K in CO{sub 2} or Ar-10%CO{sub 2}. Optical microscopy, electron probe microanalyses, and X-ray measurements on the oxide scales formed during oxidation indicate that their structures are nearly independent of temperature and the corrosion atmosphere. The scales consisted of two layers, an external one and an internal one, having a rutile (TiO{sub 2}) structure. The parabolic rate law was confirmed for growth of the external scale and the permeation depth of oxygen in titanium with apparent activation energies of 266 and 226 kJ/mol, respectively. The rate-determining diffusion species in the oxidation processes are discussed.
Sponsoring Organization:
USDOE
OSTI ID:
563590
Journal Information:
Oxidation of Metals, Journal Name: Oxidation of Metals Journal Issue: 3-4 Vol. 48; ISSN OXMEAF; ISSN 0030-770X
Country of Publication:
United States
Language:
English

Similar Records

Oxidation of Ti{sub 3}SiC{sub 2} in air
Journal Article · Tue Jul 01 00:00:00 EDT 1997 · Journal of the Electrochemical Society · OSTI ID:533123

THE OXIDATION OF HOT-PRESSED TITANIUM CARBIDE AND TITANIUM BORIDE IN THE TEMPERATURE RANGE 300-1000 C
Journal Article · Wed Dec 31 23:00:00 EST 1958 · Powder Met. · OSTI ID:4125975

High-temperature oxidation of Ti{sub 3}Al-based titanium aluminides in oxygen
Journal Article · Sat Nov 30 23:00:00 EST 1996 · Metallurgical and Materials Transactions. A, Physical Metallurgy and Materials Science · OSTI ID:438562