Temperature estimates from the zircaloy oxidation kinetics in the. cap alpha. plus. beta. phase region. [PWR; BWR]
Oxidation rates of zircaloy in steam were measured at temperatures between 961 and 1264 K and for duration times between 25 and 1900 seconds in order to calculate, in conjunction with measurements from postirradiation metallographic examination, the prior peak temperatures of zircaloy fuel rod cladding. These temperature estimates will be used in light water reactor research programs to assess (a) the accuracy of temperature measurements of fuel rod cladding peak temperatures from thermocouples attached to the surface during loss-of-coolant experiments (LOCEs), (b) the perturbation of the fuel rod cladding LOCE temperature history caused by the presence of thermocouples, and (c) the measurements of cladding azimuthal temperature gradients near thermocouple locations.
- Research Organization:
- EG and G Idaho, Inc., Idaho Falls (USA)
- DOE Contract Number:
- AC07-76ID01570
- OSTI ID:
- 5616678
- Report Number(s):
- CONF-810801-61; ON: DE82005952
- Country of Publication:
- United States
- Language:
- English
Similar Records
Temperature estimates from zircaloy oxidation kinetics and microstructures. [PWR]
Embedded Zircaloy-sheathed cladding thermocouples. [BWR; PWR]
Related Subjects
210100 -- Power Reactors
Nonbreeding
Light-Water Moderated
Boiling Water Cooled
210200 -- Power Reactors
Nonbreeding
Light-Water Moderated
Nonboiling Water Cooled
22 GENERAL STUDIES OF NUCLEAR REACTORS
220900* -- Nuclear Reactor Technology-- Reactor Safety
36 MATERIALS SCIENCE
360105 -- Metals & Alloys-- Corrosion & Erosion
ACCIDENTS
ALLOYS
BWR TYPE REACTORS
CHEMICAL REACTIONS
HIGH TEMPERATURE
LOSS OF COOLANT
MATERIALS
OXIDATION
PHASE STUDIES
PWR TYPE REACTORS
REACTOR ACCIDENTS
REACTOR MATERIALS
REACTORS
STEAM
STRESSES
TEMPERATURE DEPENDENCE
THERMAL STRESSES
TIME DEPENDENCE
TIN ALLOYS
WATER COOLED REACTORS
WATER MODERATED REACTORS
ZIRCALOY
ZIRCALOY 4
ZIRCONIUM ALLOYS
ZIRCONIUM BASE ALLOYS