Effect of small additions of silicon, iron, and aluminum on the room-temperature tensile properties of high-purity uranium

Technical Report ·
DOI:https://doi.org/10.2172/5581747· OSTI ID:5581747
Eleven binary and ternary alloys of uranium and very low concentrations of iron, silicon, and aluminum were prepared and tested for room-temperature tensile properties after various heat treatments. A yield strength approximately double that of high-purity derby uranium was obtained from a U-400 ppM Si-200 ppM Fe alloy after beta solution treatment and alpha aging. Higher silicon plus iron alloy contents resulted in increased yield strength, but showed an unacceptable loss of ductility.