Low-enriched uranium silicide dispersion fuel plates were irradiated to maximum burnups of 96% of /sup 235/U. Fuel plates containing 33 v/o U/sub 3/Si and U/sub 3/Si/sub 2/ behaved very well up to this burnup. Plates containing 33 v/o U/sub 3/Si-Al pillowed between 90 and 96% burnup of the fissile atoms. More highly loaded U/sub 3/Si-Al plates, up to 50 v/o were found to pillow at lower burnups. Plates containing 40 v/o U/sub 3/Si showed an increase swelling rate around 85% burnup. 5 refs., 10 figs.