METHOD OF PRODUCING URANIUM METAL
Patent
·
OSTI ID:4722377
The patent describes the production of a uranium fuel rod, contnining 200 to 500 ppm Fe and 500 to 1200 ppm Al, which is beta-quenched and alpha- annealed to obtain a peripheral grain structure refined by a factor of 6 to 30 from the largest initial grain size 2.0 to 3.0 mm. (NPO)
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-17-008779
- OSTI ID:
- 4722377
- Report Number(s):
- FR 1235630
- Country of Publication:
- France
- Language:
- English
Similar Records
IMPROVEMENTS IN OR RELATING TO PRODUCTION OF URANIUM METAL
HEAT TREATMENT OF DILUTE ALLOY URANIUM RODS
GRAIN REFINEMENT PRODUCED BY AN ALPHA PHASE ANNEAL OF BETA PHASE HEAT TREATED AND WATER QUENCHED URANIUM
Patent
·
Tue Mar 21 23:00:00 EST 1961
·
OSTI ID:4051540
HEAT TREATMENT OF DILUTE ALLOY URANIUM RODS
Technical Report
·
Mon May 15 00:00:00 EDT 1961
·
OSTI ID:4782792
GRAIN REFINEMENT PRODUCED BY AN ALPHA PHASE ANNEAL OF BETA PHASE HEAT TREATED AND WATER QUENCHED URANIUM
Technical Report
·
Fri Dec 31 23:00:00 EST 1954
·
OSTI ID:4785646