Studies were made of the creep properties of coldswaged and cold-swaged and base-amealed Zircaloy-2 and -3. Several differences observed in the two conditions were examined. Further work was done in an attempt to identlfy the source of inclusions found previously in some vacuum melted Zircaloy-2 after routine corrosion tests. Thls work is summarized. Results from studies of the effects of impurities on the corrosion and mechanical properties of vacuum melted Zircaloy-2 are reported. The impurities considered were Al, Cu, Mm, N, and Si. A method is described for removing residue iron contamination from Zircaloy surfaces. Zirconlum sponge and Zircaloy-2 ingotu were analyzed by fluorimetric chemistry to determine the content of naturaily occurring uranium. Results are tubulated. (For preceding period see WAPD-ZH-10.) (D.E.B.)
Research Organization:
Westinghouse Electric Corp. Bettis Plant, Pittsburgh
DOE Contract Number:
AT(11-1)-GEN-14
NSA Number:
NSA-13-001397
OSTI ID:
4327331
Report Number(s):
WAPD-ZH-11
Country of Publication:
United States
Language:
English

Similar Records

ZIRCONIUM HIGHLIGHTS, APRIL 1958
Technical Report · Thu Oct 30 23:00:00 EST 1958 · OSTI ID:4327146

ZIRCONIUM HIGHLIGHTS
Technical Report · Mon Jun 01 00:00:00 EDT 1959 · OSTI ID:4227697

ZIRCONIUM HIGHLIGHTS
Technical Report · Tue Jul 01 00:00:00 EDT 1958 · OSTI ID:4313425