CLEAVAGE FRACTURE IN A Cr-Ni-Mo STEEL
Journal Article
·
· Sbornik Statei Ural' Zavod Tyazh. Mashinostroeniya im. S. Ordzhonikidze
OSTI ID:4195016
In order to evaluate the effect of technological factors of smelting and casting on the susceptibility of Cr-NiMo steel 34KhNZM io cleavage fracture (CF), six forgings were investigated. The investigations dealt with the following factors: macro and microstructure, the nature of ihe fracture, incidence of nonmetallic inclusions, and the mechanical properties of the forgings. It was established ihat CF is observed only in the upper and central portions of the forgings and that it is independent of the concentration of nonmetallic inclusions and gases in the steel. CF is caused by a coarse dendritic structure which had formed as a result of excessively high casting temperatures and which was not refined in the course of forging.
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-14-000674
- OSTI ID:
- 4195016
- Journal Information:
- Sbornik Statei Ural' Zavod Tyazh. Mashinostroeniya im. S. Ordzhonikidze, Journal Name: Sbornik Statei Ural' Zavod Tyazh. Mashinostroeniya im. S. Ordzhonikidze Vol. Vol: No. 5
- Country of Publication:
- Country unknown/Code not available
- Language:
- English
Similar Records
Influence of nonmetallic inclusions on the character of fracture of 20GFL steel
Cleavage fracture of microalloyed forging steels
Intergranular fracture of low-alloy cast steel
Journal Article
·
Fri Feb 28 23:00:00 EST 1986
· Met. Sci. Heat Treat. Met. (Engl. Transl.); (United States)
·
OSTI ID:5474637
Cleavage fracture of microalloyed forging steels
Journal Article
·
Tue Jan 31 23:00:00 EST 1995
· Scripta Metallurgica et Materialia
·
OSTI ID:231114
Intergranular fracture of low-alloy cast steel
Journal Article
·
Wed Jan 31 23:00:00 EST 1996
· Materials Characterization
·
OSTI ID:260357