THERMAL CONDUCTIVITY OF ALUMINUM-LITHIUM ALLOYS CONTAINING UP TO 8% LITHIUM
The thermal conductivities of Al-Li alloys containing up to 8 wt.% lithium were determined at 125 to 260 deg C. The addition of lithium to aluminum sharply reduces the conductivity from 0.60 cal/(sec) deg C)(cm) for pure aluminum to 0.22 cal/(sec)( deg C)(cm) for 2 wt.% alloys; further addition linearly and more gradually decreases the conductivity to 0.16 cal/(sec)( deg C)(cm) for a 7.9 wt.% alloy. (auth)
- Research Organization:
- Du Pont de Nemours (E.I.) & Co. Savannah River Lab., Aiken, S.C.
- DOE Contract Number:
- AT(07-2)-1
- NSA Number:
- NSA-15-001826
- OSTI ID:
- 4132227
- Report Number(s):
- DP-463
- Resource Relation:
- Other Information: Decl. Aug. 4, 1960. Orig. Receipt Date: 31-DEC-61
- Country of Publication:
- United States
- Language:
- English
Similar Records
CREEP OF ALUMINUM-LITHIUM ALLOY
RELATION BETWEEN MICROSTRUCTURE AND THERMAL CONDUCTIVITY IN ALUMINUM- URANIUM ALLOYS
PROPERTIES OF URANIUM CARBIDES
Technical Report
·
Sun Oct 01 00:00:00 EDT 1961
·
OSTI ID:4132227
RELATION BETWEEN MICROSTRUCTURE AND THERMAL CONDUCTIVITY IN ALUMINUM- URANIUM ALLOYS
Journal Article
·
Tue Jan 01 00:00:00 EST 1963
· Can. Met. Quart.
·
OSTI ID:4132227
+1 more
PROPERTIES OF URANIUM CARBIDES
Journal Article
·
Sat Sep 15 00:00:00 EDT 1962
· American Ceramic Society Bulletin (U.S.)
·
OSTI ID:4132227