Title: Electrical properties of GaAs metal–oxide–semiconductor structure comprising Al{sub 2}O{sub 3} gate oxide and AlN passivation layer fabricated in situ using a metal–organic vapor deposition/atomic layer deposition hybrid system

Abstract

This paper presents a compressive study on the fabrication and optimization of GaAs metal–oxide–semiconductor (MOS) structures comprising a Al{sub 2}O{sub 3} gate oxide, deposited via atomic layer deposition (ALD), with an AlN interfacial passivation layer prepared in situ via metal–organic chemical vapor deposition (MOCVD). The established protocol afforded self-limiting growth of Al{sub 2}O{sub 3} in the atmospheric MOCVD reactor. Consequently, this enabled successive growth of MOCVD-formed AlN and ALD-formed Al{sub 2}O{sub 3} layers on the GaAs substrate. The effects of AlN thickness, post-deposition anneal (PDA) conditions, and crystal orientation of the GaAs substrate on the electrical properties of the resulting MOS capacitors were investigated. Thin AlN passivation layers afforded incorporation of optimum amounts of nitrogen, leading to good capacitance–voltage (C–V) characteristics with reduced frequency dispersion. In contrast, excessively thick AlN passivation layers degraded the interface, thereby increasing the interfacial density of states (D{sub it}) near the midgap and reducing the conduction band offset. To further improve the interface with the thin AlN passivation layers, the PDA conditions were optimized. Using wet nitrogen at 600 °C was effective to reduce D{sub it} to below 2 × 10{sup 12} cm{sup −2} eV{sup −1}. Using a (111)A substrate was also effective in reducingmore » the frequency dispersion of accumulation capacitance, thus suggesting the suppression of traps in GaAs located near the dielectric/GaAs interface. The current findings suggest that using an atmosphere ALD process with in situ AlN passivation using the current MOCVD system could be an efficient solution to improving GaAs MOS interfaces.« less

Authors:
; ; ; ; ;  [1]
  1. Sumitomo Chemical Co., Ltd., IT-related Chemicals Research Laboratory, 6 Kitahara, Tsukuba, Ibaraki 300-3294 (Japan)
Publication Date:
OSTI Identifier:
22492319
Resource Type:
Journal Article
Journal Name:
AIP Advances
Additional Journal Information:
Journal Volume: 5; Journal Issue: 8; Other Information: (c) 2015 Author(s); Country of input: International Atomic Energy Agency (IAEA); Journal ID: ISSN 2158-3226
Country of Publication:
United States
Language:
English
Subject:
36 MATERIALS SCIENCE; ALUMINIUM NITRIDES; ALUMINIUM OXIDES; CAPACITANCE; CHEMICAL VAPOR DEPOSITION; CRYSTALS; DENSITY OF STATES; DEPOSITS; DIELECTRIC MATERIALS; ELECTRIC POTENTIAL; EV RANGE; FABRICATION; GALLIUM ARSENIDES; INTERFACES; LAYERS; NITROGEN; PASSIVATION; SEMICONDUCTOR MATERIALS; SILICON OXIDES; SUBSTRATES; TRAPS

Citation Formats

Aoki, Takeshi, Fukuhara, Noboru, Osada, Takenori, Sazawa, Hiroyuki, Hata, Masahiko, and Inoue, Takayuki. Electrical properties of GaAs metal–oxide–semiconductor structure comprising Al{sub 2}O{sub 3} gate oxide and AlN passivation layer fabricated in situ using a metal–organic vapor deposition/atomic layer deposition hybrid system. United States: N. p., 2015. Web. doi:10.1063/1.4929371.
Aoki, Takeshi, Fukuhara, Noboru, Osada, Takenori, Sazawa, Hiroyuki, Hata, Masahiko, & Inoue, Takayuki. Electrical properties of GaAs metal–oxide–semiconductor structure comprising Al{sub 2}O{sub 3} gate oxide and AlN passivation layer fabricated in situ using a metal–organic vapor deposition/atomic layer deposition hybrid system. United States. https://doi.org/10.1063/1.4929371
Aoki, Takeshi, Fukuhara, Noboru, Osada, Takenori, Sazawa, Hiroyuki, Hata, Masahiko, and Inoue, Takayuki. Sat . "Electrical properties of GaAs metal–oxide–semiconductor structure comprising Al{sub 2}O{sub 3} gate oxide and AlN passivation layer fabricated in situ using a metal–organic vapor deposition/atomic layer deposition hybrid system". United States. https://doi.org/10.1063/1.4929371.
@article{osti_22492319,
title = {Electrical properties of GaAs metal–oxide–semiconductor structure comprising Al{sub 2}O{sub 3} gate oxide and AlN passivation layer fabricated in situ using a metal–organic vapor deposition/atomic layer deposition hybrid system},
author = {Aoki, Takeshi and Fukuhara, Noboru and Osada, Takenori and Sazawa, Hiroyuki and Hata, Masahiko and Inoue, Takayuki},
abstractNote = {This paper presents a compressive study on the fabrication and optimization of GaAs metal–oxide–semiconductor (MOS) structures comprising a Al{sub 2}O{sub 3} gate oxide, deposited via atomic layer deposition (ALD), with an AlN interfacial passivation layer prepared in situ via metal–organic chemical vapor deposition (MOCVD). The established protocol afforded self-limiting growth of Al{sub 2}O{sub 3} in the atmospheric MOCVD reactor. Consequently, this enabled successive growth of MOCVD-formed AlN and ALD-formed Al{sub 2}O{sub 3} layers on the GaAs substrate. The effects of AlN thickness, post-deposition anneal (PDA) conditions, and crystal orientation of the GaAs substrate on the electrical properties of the resulting MOS capacitors were investigated. Thin AlN passivation layers afforded incorporation of optimum amounts of nitrogen, leading to good capacitance–voltage (C–V) characteristics with reduced frequency dispersion. In contrast, excessively thick AlN passivation layers degraded the interface, thereby increasing the interfacial density of states (D{sub it}) near the midgap and reducing the conduction band offset. To further improve the interface with the thin AlN passivation layers, the PDA conditions were optimized. Using wet nitrogen at 600 °C was effective to reduce D{sub it} to below 2 × 10{sup 12} cm{sup −2} eV{sup −1}. Using a (111)A substrate was also effective in reducing the frequency dispersion of accumulation capacitance, thus suggesting the suppression of traps in GaAs located near the dielectric/GaAs interface. The current findings suggest that using an atmosphere ALD process with in situ AlN passivation using the current MOCVD system could be an efficient solution to improving GaAs MOS interfaces.},
doi = {10.1063/1.4929371},
url = {https://www.osti.gov/biblio/22492319}, journal = {AIP Advances},
issn = {2158-3226},
number = 8,
volume = 5,
place = {United States},
year = {2015},
month = {8}
}