Surface smoothing effect of an amorphous thin film deposited by atomic layer deposition on a surface with nano-sized roughness
- Zhejiang University, Department of Information Science and Electronic Engineering, No. 38 Zheda Road, Hangzhou 310027 (China)
- Zhejiang University, Department of Materials Science and Engineering, No. 38 Zheda Road, Hangzhou 310027 (China)
Previously, Lau (one of the authors) pointed out that the deposition of an amorphous thin film by atomic layer deposition (ALD) on a substrate with nano-sized roughness probably has a surface smoothing effect. In this letter, polycrystalline zinc oxide deposited by ALD onto a smooth substrate was used as a substrate with nano-sized roughness. Atomic force microscopy (AFM) and cross-sectional transmission electron microscopy (XTEM) were used to demonstrate that an amorphous aluminum oxide thin film deposited by ALD can reduce the surface roughness of a polycrystalline zinc oxide coated substrate.
- OSTI ID:
- 22251226
- Journal Information:
- AIP Advances, Vol. 4, Issue 2; Other Information: (c) 2014 Author(s); Country of input: International Atomic Energy Agency (IAEA); ISSN 2158-3226
- Country of Publication:
- United States
- Language:
- English
Similar Records
Atomically Smooth Surfaces as Substrates for Advanced Neutron Supermirrors
Structure evolution of zinc oxide thin films deposited by unbalance DC magnetron sputtering
Toward Ideal Metal–Organic Framework Thin-Film Growth via Automated Layer-by-Layer Deposition: Examples Based on Perylene Diimide Linkers
Technical Report
·
Thu Nov 02 00:00:00 EDT 2023
·
OSTI ID:22251226
Structure evolution of zinc oxide thin films deposited by unbalance DC magnetron sputtering
Journal Article
·
Tue Apr 19 00:00:00 EDT 2016
· AIP Conference Proceedings
·
OSTI ID:22251226
+3 more
Toward Ideal Metal–Organic Framework Thin-Film Growth via Automated Layer-by-Layer Deposition: Examples Based on Perylene Diimide Linkers
Journal Article
·
Tue Oct 25 00:00:00 EDT 2022
· Chemistry of Materials
·
OSTI ID:22251226
+9 more