Nanoindentation study of bulk zirconium hydrides at elevated temperatures

Journal Article · · Journal of Alloys and Compounds
 [1];  [2];  [1];  [3];  [1]
  1. Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States)
  2. Univ. of California, Berkeley, CA (United States)
  3. Oak Ridge National Lab. (ORNL), Oak Ridge, TN (United States); Michigan State Univ., East Lansing, MI (United States)

Here, the mechanical properties of zirconium hydrides was studied using nano-indentation technique at a temperature range of 25 – 400 °C. Temperature dependency of reduced elastic modulus and hardness of δ- and ε-zirconium hydrides were obtained by conducting nanoindentation experiments on the bulk hydride samples with independently heating capability of indenter and heating stage. The reduced elastic modulus of δ-zirconium hydride (H/Zr ratio =1.61) decreased from ~113 GPa to ~109 GPa while temperature increased from room temperature to 400°C. For ε-zirconium hydrides (H/Zr ratio=1.79), the reduced elastic modulus decreased from 61 GPa to 54 GPa as temperature increased from room temperature to 300 °C. Whereas, hardness of δ-zirconium hydride significantly decreased from 4.1 GPa to 2.41 GPa when temperature increased from room temperature to 400 °C. Similarly, hardness of ε-zirconium hydride decreased from 3.06 GPa to 2.19 GPa with temperature increase from room temperature to 300°C.

Research Organization:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN (United States)
Sponsoring Organization:
USDOE Office of Nuclear Energy (NE)
Grant/Contract Number:
AC05-00OR22725
OSTI ID:
1400216
Alternate ID(s):
OSTI ID: 1549610
Journal Information:
Journal of Alloys and Compounds, Journal Name: Journal of Alloys and Compounds Journal Issue: C Vol. 726; ISSN 0925-8388
Publisher:
ElsevierCopyright Statement
Country of Publication:
United States
Language:
English

Similar Records

Depth Dependence of the Mechanical Properties of Human Enamel by Nanoindentation
Journal Article · Thu Feb 16 23:00:00 EST 2006 · Journal of Biomedical Materials Research Part A, vol. 81A, no. 1, April 1, 2007, pp. 66-74 · OSTI ID:919219

Influence of sintering temperatures on hardness and Young's modulus of tricalcium phosphate bioceramic by nanoindentation technique
Journal Article · Thu Jul 15 00:00:00 EDT 2004 · Materials Characterization · OSTI ID:20748636

High-Throughput Nanoindentation Mapping of Additively Manufactured T91 Steel
Journal Article · Thu Mar 03 23:00:00 EST 2022 · JOM. Journal of the Minerals, Metals & Materials Society · OSTI ID:1873342