Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route
Abstract
Layered oxide LiNixMnyCozO2 (NMC) cathodes are often synthesized as polycrystalline secondary particles. Due to intergranular fracture stemming from volume changes of randomly oriented primary particles during charge/discharge, the synthesis of larger single-crystalline cathodes is of high interest. In this work, molten salt assisted growth of micron-sized Ni-rich crystals is achieved with excellent crystallinity, low cation mixing, and negligible impurities. However, electrochemical performance is compromised by high surface reactivity resulting in decomposition of electrolyte and subsequent formation of a thick CEI layer. While intergranular fracture is eliminated, planar gliding and severe intragranular fracture along the (003) plane occurs in the high voltage region within the first few cycles and is associated primarily with H2 to H3 structural transitions. In addition, H2 to H3 transitions are highly irreversible with cyclic voltammograms revealing polarization growth within <5 cycles. Subsequently, the single-crystalline material exhibited markedly reduced available capacity and enhanced capacity fade from sharp impedance growth compared to its polycrystalline counterpart. Here, this work furthers a fundamental understanding into the limitations of single-crystalline Ni-rich cathodes, and the obstacles limiting the advantages offered by the single-crystalline morphology.
- Authors:
-
- Worcester Polytechnic Institute, MA (United States)
- Argonne National Lab. (ANL), Lemont, IL (United States)
- Rice Univ., Houston, TX (United States)
- Publication Date:
- Research Org.:
- Argonne National Laboratory (ANL), Argonne, IL (United States)
- Sponsoring Org.:
- USDOE Office of Energy Efficiency and Renewable Energy (EERE); Ford Motor Company
- OSTI Identifier:
- 1902347
- Grant/Contract Number:
- AC02-06CH11357
- Resource Type:
- Accepted Manuscript
- Journal Name:
- Journal of Power Sources
- Additional Journal Information:
- Journal Volume: 545; Journal ID: ISSN 0378-7753
- Publisher:
- Elsevier
- Country of Publication:
- United States
- Language:
- English
- Subject:
- 25 ENERGY STORAGE; Li-ion battery; LiNi0.8Mn0.1Co0.1O; NMC; Single-crystal; intragranular fracture
Citation Formats
Azhari, Luqman, Meng, Zifei, Yang, Zhenzhen, Gao, Guanhui, Han, Yimo, and Wang, Yan. Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route. United States: N. p., 2022.
Web. doi:10.1016/j.jpowsour.2022.231963.
Azhari, Luqman, Meng, Zifei, Yang, Zhenzhen, Gao, Guanhui, Han, Yimo, & Wang, Yan. Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route. United States. https://doi.org/10.1016/j.jpowsour.2022.231963
Azhari, Luqman, Meng, Zifei, Yang, Zhenzhen, Gao, Guanhui, Han, Yimo, and Wang, Yan. Wed .
"Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route". United States. https://doi.org/10.1016/j.jpowsour.2022.231963. https://www.osti.gov/servlets/purl/1902347.
@article{osti_1902347,
title = {Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route},
author = {Azhari, Luqman and Meng, Zifei and Yang, Zhenzhen and Gao, Guanhui and Han, Yimo and Wang, Yan},
abstractNote = {Layered oxide LiNixMnyCozO2 (NMC) cathodes are often synthesized as polycrystalline secondary particles. Due to intergranular fracture stemming from volume changes of randomly oriented primary particles during charge/discharge, the synthesis of larger single-crystalline cathodes is of high interest. In this work, molten salt assisted growth of micron-sized Ni-rich crystals is achieved with excellent crystallinity, low cation mixing, and negligible impurities. However, electrochemical performance is compromised by high surface reactivity resulting in decomposition of electrolyte and subsequent formation of a thick CEI layer. While intergranular fracture is eliminated, planar gliding and severe intragranular fracture along the (003) plane occurs in the high voltage region within the first few cycles and is associated primarily with H2 to H3 structural transitions. In addition, H2 to H3 transitions are highly irreversible with cyclic voltammograms revealing polarization growth within <5 cycles. Subsequently, the single-crystalline material exhibited markedly reduced available capacity and enhanced capacity fade from sharp impedance growth compared to its polycrystalline counterpart. Here, this work furthers a fundamental understanding into the limitations of single-crystalline Ni-rich cathodes, and the obstacles limiting the advantages offered by the single-crystalline morphology.},
doi = {10.1016/j.jpowsour.2022.231963},
journal = {Journal of Power Sources},
number = ,
volume = 545,
place = {United States},
year = {Wed Aug 17 00:00:00 EDT 2022},
month = {Wed Aug 17 00:00:00 EDT 2022}
}
Works referenced in this record:
Single-crystal based studies for correlating the properties and high-voltage performance of Li[Ni x Mn y Co 1−x−y ]O 2 cathodes
journal, January 2019
- Zhu, Jian; Chen, Guoying
- Journal of Materials Chemistry A, Vol. 7, Issue 10
Breaking Free from Cobalt Reliance in Lithium-Ion Batteries
journal, September 2020
- Gourley, Storm William D.; Or, Tyler; Chen, Zhongwei
- iScience, Vol. 23, Issue 9
A perspective on single-crystal layered oxide cathodes for lithium-ion batteries
journal, May 2021
- Langdon, Jayse; Manthiram, Arumugam
- Energy Storage Materials, Vol. 37
Effect of Particle Size on LiNi0.6Mn0.2Co0.2O2 Layered Oxide Performance in Li-Ion Batteries
journal, May 2022
- Soloy, Adrien; Flahaut, Delphine; Allouche, Joachim
- ACS Applied Energy Materials, Vol. 5, Issue 5
Mechanical properties of cathode materials for lithium-ion batteries
journal, May 2022
- Stallard, Joe C.; Wheatcroft, Laura; Booth, Samuel G.
- Joule, Vol. 6, Issue 5
Simultaneous Enhancement of Interfacial Stability and Kinetics of Single-Crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 through Optimized Surface Coating and Doping
journal, November 2020
- Bao, Wenda; Qian, Guannan; Zhao, Lianqi
- Nano Letters, Vol. 20, Issue 12
Improved Cycling Stability of Li[Ni 0.90 Co 0.05 Mn 0.05 ]O 2 Through Microstructure Modification by Boron Doping for Li-Ion Batteries
journal, July 2018
- Park, Kang-Joon; Jung, Hun-Gi; Kuo, Liang-Yin
- Advanced Energy Materials, Vol. 8, Issue 25
Surface-Modified Quaternary Layered Ni-Rich Cathode Materials by Li2ZrO3 for Improved Electrochemical Performance for High-Power Li-Ion Batteries
journal, April 2022
- Jeyakumar, Juliya; Wu, Yi-Shiuan; Wu, She-Huang
- ACS Applied Energy Materials, Vol. 5, Issue 4
Targeted Surface Doping with Reversible Local Environment Improves Oxygen Stability at the Electrochemical Interfaces of Nickel-Rich Cathode Materials
journal, October 2019
- Steiner, James D.; Cheng, Hao; Walsh, Julia
- ACS Applied Materials & Interfaces, Vol. 11, Issue 41
Modified Nickel-Rich Cathodes via Conformal Nanoparticle Coating of Precursors Using a Single Reactor Process
journal, December 2021
- Azhari, Luqman; Arsenault, Renata; Gao, Guanhui
- ACS Applied Energy Materials, Vol. 4, Issue 12
Controlling Ni2+ from the Surface to the Bulk by a New Cathode Electrolyte Interphase Formation on a Ni-Rich Layered Cathode in High-Safe and High-Energy-Density Lithium-Ion Batteries
journal, February 2021
- Yeh, Nan-Hung; Wang, Fu-Ming; Khotimah, Chusnul
- ACS Applied Materials & Interfaces, Vol. 13, Issue 6
Comprehensive Study of Al- and Zr-Modified LiNi 0.8 Mn 0.1 Co 0.1 O 2 through Synergy of Coating and Doping
journal, August 2020
- Gao, Yan; Park, Jonghyun; Liang, Xinhua
- ACS Applied Energy Materials, Vol. 3, Issue 9
Activation Mechanism of LiNi 0.80 Co 0.15 Al 0.05 O 2 : Surface and Bulk Operando Electrochemical, Differential Electrochemical Mass Spectrometry, and X-ray Diffraction Analyses
journal, January 2015
- Robert, Rosa; Bünzli, Christa; Berg, Erik J.
- Chemistry of Materials, Vol. 27, Issue 2
Designing principle for Ni-rich cathode materials with high energy density for practical applications
journal, July 2018
- Xia, Yu; Zheng, Jianming; Wang, Chongmin
- Nano Energy, Vol. 49
Interfacial Origin of Performance Improvement and Fade for 4.6 V LiNi 0.5 Co 0.2 Mn 0.3 O 2 Battery Cathodes
journal, May 2014
- Lee, Yu-Mi; Nam, Kyoung-Mo; Hwang, Eui-Hyung
- The Journal of Physical Chemistry C, Vol. 118, Issue 20
Revealing the degradation mechanism of Ni-rich cathode materials after ambient storage and related regeneration method
journal, January 2021
- Lv, Congjie; Li, Zhenguo; Ren, Xiaoning
- Journal of Materials Chemistry A, Vol. 9, Issue 7
Nasicon-Type Surface Functional Modification in Core–Shell LiNi 0.5 Mn 0.3 Co 0.2 O 2 @NaTi 2 (PO 4 ) 3 Cathode Enhances Its High-Voltage Cycling Stability and Rate Capacity toward Li-Ion Batteries
journal, January 2018
- Liang, Longwei; Sun, Xuan; Wu, Chen
- ACS Applied Materials & Interfaces, Vol. 10, Issue 6
Demonstrating Apparently Inconspicuous but Sensitive Impacts on the Rollover Failure of Lithium-Ion Batteries at a High Voltage
journal, November 2021
- Klein, Sven; Bärmann, Peer; Stolz, Lukas
- ACS Applied Materials & Interfaces, Vol. 13, Issue 48
Changing Established Belief on Capacity Fade Mechanisms: Thorough Investigation of LiNi 1/3 Co 1/3 Mn 1/3 O 2 (NCM111) under High Voltage Conditions
journal, January 2017
- Kasnatscheew, Johannes; Evertz, Marco; Streipert, Benjamin
- The Journal of Physical Chemistry C, Vol. 121, Issue 3
Research Progress of Single‐Crystal Nickel‐Rich Cathode Materials for Lithium Ion Batteries
journal, July 2021
- You, Bianzheng; Wang, Zhixing; Shen, Fang
- Small Methods, Vol. 5, Issue 8
Powder Characteristics of Pb(Mg1/3Nb2/3)O3 Prepared by Molten Salt Synthesis
journal, May 1993
- Yoon, Ki Hyun; Cho, Yong-Soo; Lee, Dong-Heon
- Journal of the American Ceramic Society, Vol. 76, Issue 5
Degradation and Aging Routes of Ni-Rich Cathode Based Li-Ion Batteries
journal, January 2020
- Teichert, Philipp; Eshetu, Gebrekidan Gebresilassie; Jahnke, Hannes
- Batteries, Vol. 6, Issue 1
Quantitative analysis of Ni2+/Ni3+ in Li[NixMnyCoz]O2 cathode materials: Non-linear least-squares fitting of XPS spectra
journal, May 2018
- Fu, Zewei; Hu, Juntao; Hu, Wenlong
- Applied Surface Science, Vol. 441
Comparison of Single Crystal and Polycrystalline LiNi 0.5 Mn 0.3 Co 0.2 O 2 Positive Electrode Materials for High Voltage Li-Ion Cells
journal, January 2017
- Li, Jing; Cameron, Andrew R.; Li, Hongyang
- Journal of The Electrochemical Society, Vol. 164, Issue 7
Synthesis of Single Crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 with Enhanced Electrochemical Performance for Lithium Ion Batteries
journal, January 2018
- Li, Hongyang; Li, Jing; Ma, Xiaowei
- Journal of The Electrochemical Society, Vol. 165, Issue 5
Effect of Lithiation upon the Shear Strength of NMC811 Single Crystals
journal, April 2022
- Stallard, Joe C.; Vema, Sundeep; Hall, David S.
- Journal of The Electrochemical Society, Vol. 169, Issue 4
Synthesis of Single Crystal LiNi 0.88 Co 0.09 Al 0.03 O 2 with a Two-Step Lithiation Method
journal, January 2019
- Li, Hongyang; Li, Jing; Zaker, Nafiseh
- Journal of The Electrochemical Society, Vol. 166, Issue 10
Single-crystal nickel-rich layered-oxide battery cathode materials: synthesis, electrochemistry, and intra-granular fracture
journal, May 2020
- Qian, Guannan; Zhang, Youtian; Li, Linsen
- Energy Storage Materials, Vol. 27
Mechanical and physical properties of LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC)
journal, August 2017
- Cheng, Eric Jianfeng; Hong, Kicheol; Taylor, Nathan John
- Journal of the European Ceramic Society, Vol. 37, Issue 9
From Coating to Dopant: How the Transition Metal Composition Affects Alumina Coatings on Ni-Rich Cathodes
journal, November 2017
- Han, Binghong; Key, Baris; Lapidus, Saul H.
- ACS Applied Materials & Interfaces, Vol. 9, Issue 47
Degradation Mechanism of Ni-Enriched NCA Cathode for Lithium Batteries: Are Microcracks Really Critical?
journal, May 2019
- Park, Kang-Joon; Hwang, Jang-Yeon; Ryu, Hoon-Hee
- ACS Energy Letters, Vol. 4, Issue 6
Bulk fatigue induced by surface reconstruction in layered Ni-rich cathodes for Li-ion batteries
journal, August 2020
- Xu, Chao; Märker, Katharina; Lee, Juhan
- Nature Materials, Vol. 20, Issue 1
The cathode–electrolyte interface in the Li-ion battery
journal, November 2004
- Edström, K.; Gustafsson, T.; Thomas, J. O.
- Electrochimica Acta, Vol. 50, Issue 2-3
Lithium Nickel Cobalt Manganese Oxide Synthesized Using Alkali Chloride Flux: Morphology and Performance As a Cathode Material for Lithium Ion Batteries
journal, April 2012
- Kim, Yongseon
- ACS Applied Materials & Interfaces, Vol. 4, Issue 5
All-Dry Synthesis of Single Crystal NMC Cathode Materials for Li-Ion Batteries
journal, October 2020
- Zheng, Lituo; Bennett, J. Craig; Obrovac, M. N.
- Journal of The Electrochemical Society, Vol. 167, Issue 13
On the Sensitivity of the Ni-rich Layered Cathode Materials for Li-ion Batteries to the Different Calcination Conditions
journal, October 2020
- Ronduda, Hubert; Zybert, Magdalena; Szczęsna-Chrzan, Anna
- Nanomaterials, Vol. 10, Issue 10
Oxygen Anion Solubility as a Factor in Molten Flux Crystal Growth, Synthesis, and Characterization of Four New Reduced Lanthanide Molybdenum Oxides: Ce4.918(3)Mo3O16, Pr4.880(3)Mo3O16, Nd4.910(3)Mo3O16, and Sm4.952(3)Mo3O16
journal, July 2016
- Cortese, Anthony J.; Abeysinghe, Dileka; Wilkins, Branford
- Crystal Growth & Design, Vol. 16, Issue 8
Growth Manner of Octahedral-Shaped Li(Ni 1/3 Co 1/3 Mn 1/3 )O 2 Single Crystals in Molten Na 2 SO 4
journal, April 2016
- Kimijima, Takeshi; Zettsu, Nobuyuki; Teshima, Katsuya
- Crystal Growth & Design, Vol. 16, Issue 5
High Performance Cathode Recovery from Different Electric Vehicle Recycling Streams
journal, September 2018
- Zheng, Zhangfeng; Chen, Mengyuan; Wang, Qiang
- ACS Sustainable Chemistry & Engineering, Vol. 6, Issue 11
Polycrystalline and Single Crystalline NCM Cathode Materials—Quantifying Particle Cracking, Active Surface Area, and Lithium Diffusion
journal, March 2021
- Trevisanello, Enrico; Ruess, Raffael; Conforto, Gioele
- Advanced Energy Materials, Vol. 11, Issue 18
Tuning Cobalt‐Free Nickel‐Rich Layered LiNi0.9Mn0.1O2Cathode Material for Lithium‐Ion Batteries
journal, June 2020
- Ma, Rui; Zhao, Zhikun; Fu, Jiale
- ChemElectroChem, Vol. 7, Issue 12
Understanding fundamental effects of Cu impurity in different forms for recovered LiNi0.6Co0.2Mn0.2O2 cathode materials
journal, December 2020
- Zhang, Ruihan; Meng, Zifei; Ma, Xiaotu
- Nano Energy, Vol. 78
Stabilizing nickel-rich layered oxide cathodes by magnesium doping for rechargeable lithium-ion batteries
journal, January 2019
- Li, Hang; Zhou, Pengfei; Liu, Fangming
- Chemical Science, Vol. 10, Issue 5
Evaluating single-crystal and polycrystalline NMC811 electrodes in lithium-ion cells via non-destructive EIS alone
journal, May 2022
- Saunders, Luke; Wang, Jiabin; Stimming, Ulrich
- Journal of Applied Electrochemistry, Vol. 52, Issue 9
Surface regulation enables high stability of single-crystal lithium-ion cathodes at high voltage
journal, June 2020
- Zhang, Fang; Lou, Shuaifeng; Li, Shuang
- Nature Communications, Vol. 11, Issue 1
Building Safe Lithium-Ion Batteries for Electric Vehicles: A Review
journal, December 2019
- Duan, Jian; Tang, Xuan; Dai, Haifeng
- Electrochemical Energy Reviews, Vol. 3, Issue 1
A universal etching method for synthesizing high-performance single crystal cathode materials
journal, September 2021
- Ma, Xiaotu; Vanaphuti, Panawan; Fu, Jinzhao
- Nano Energy, Vol. 87
Reversible planar gliding and microcracking in a single-crystalline Ni-rich cathode
journal, December 2020
- Bi, Yujing; Tao, Jinhui; Wu, Yuqin
- Science, Vol. 370, Issue 6522
Next‐Generation Cobalt‐Free Cathodes – A Prospective Solution to the Battery Industry's Cobalt Problem
journal, January 2022
- Muralidharan, Nitin; Self, Ethan C.; Dixit, Marm
- Advanced Energy Materials, Vol. 12, Issue 9
Revealing Mechanism of Li 3 PO 4 Coating Suppressed Surface Oxygen Release for Commercial Ni-Rich Layered Cathodes
journal, July 2020
- Gan, Qingmeng; Qin, Ning; Wang, Zhenyu
- ACS Applied Energy Materials, Vol. 3, Issue 8
Evolution of Structure and Lithium Dynamics in LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) Cathodes during Electrochemical Cycling
journal, March 2019
- Märker, Katharina; Reeves, Philip J.; Xu, Chao
- Chemistry of Materials, Vol. 31, Issue 7
Assessing Long‐Term Cycling Stability of Single‐Crystal Versus Polycrystalline Nickel‐Rich NCM in Pouch Cells with 6 mAh cm
−2
Electrodes
journal, February 2022
- Zhao, Wengao; Zou, Lianfeng; Zhang, Leiting
- Small, Vol. 18, Issue 14
In situ inorganic conductive network formation in high-voltage single-crystal Ni-rich cathodes
journal, September 2021
- Fan, Xinming; Ou, Xing; Zhao, Wengao
- Nature Communications, Vol. 12, Issue 1
Bulk and surface degradation in layered Ni-rich cathode for Li ions batteries: Defect proliferation via chain reaction mechanism
journal, March 2021
- Yang, Chengkai; Shao, Ruiwen; Wang, Qian
- Energy Storage Materials, Vol. 35
Prospects and limitations of single-crystal cathode materials to overcome cross-talk phenomena in high-voltage lithium ion cells
journal, January 2021
- Klein, Sven; Bärmann, Peer; Fromm, Olga
- Journal of Materials Chemistry A, Vol. 9, Issue 12
Superior Cycle Stability of Single Crystal Nickel-Rich Layered Oxides with Micron-Scale Grain Size as Cathode Material for Lithium Ion Batteries
journal, June 2020
- Yang, Cheng
- International Journal of Electrochemical Science
Effects of Alkali Cations and Sulfate/Chloride Anions on the Flux Growth of {001}-Faceted β-Li2TiO3 Crystals
journal, January 2017
- Xiao, Xiong; Hayashi, Fumitaka; Yubuta, Kunio
- Crystal Growth & Design, Vol. 17, Issue 3
Reaction Heterogeneity in LiNi 0.8 Co 0.15 Al 0.05 O 2 Induced by Surface Layer
journal, August 2017
- Grenier, Antonin; Liu, Hao; Wiaderek, Kamila M.
- Chemistry of Materials, Vol. 29, Issue 17
Automotive Li-Ion Batteries: Current Status and Future Perspectives
journal, January 2019
- Ding, Yuanli; Cano, Zachary P.; Yu, Aiping
- Electrochemical Energy Reviews, Vol. 2, Issue 1
Temperature-Swing Synthesis of Large-Size Single-Crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode Materials
journal, January 2021
- Qian, Guannan; Li, Zhiyuan; Meng, Dechao
- Journal of The Electrochemical Society, Vol. 168, Issue 1
Tuning the Li/Ni Disorder of the NMC811 Cathode by Thermally Driven Competition between Lattice Ordering and Structure Decomposition
journal, February 2020
- Wang, Ting; Ren, Keliang; Xiao, Wei
- The Journal of Physical Chemistry C, Vol. 124, Issue 10
Minimization of the cation mixing in Li1+x(NMC)1−xO2 as cathode material
journal, March 2010
- Zhang, Xiaoyu; Jiang, W. J.; Mauger, A.
- Journal of Power Sources, Vol. 195, Issue 5