VALIDATION FOR THE PERMANGANATE DIGESTION OF REILLEX HPQ ANION RESIN
The flowsheet for the digestion of Reillex{trademark} HPQ was validated both under the traditional alkaline conditions and under strongly acidic conditions. Due to difficulty in performing a pH adjustment in the large tank where this flowsheet must be performed, the recommended digestion conditions were changed from pH 8-10 to 8 M HNO{sub 3}. Thus, no pH adjustment of the solution is required prior to performing the permanganate addition and digestion and the need to sample the digestion tank to confirm appropriate pH range for digestion may be avoided. Neutralization of the acidic digestion solution will be performed after completion of the resin digestion cycle. The amount of permanganate required for this type of resin (Reillex{trademark} HPQ) was increased from 1 kg/L resin to 4 kg/L resin to reduce the amount of residual resin solids to a minimal amount (<5%). The length of digestion time at 70 C remains unchanged at 15 hours. These parameters are not optimized but are expected to be adequate for the conditions. The flowsheet generates a significant amount of fine manganese dioxide (MnO{sub 2}) solids (1.71 kg/L resin) and involves the generation of a significant liquid volume due to the low solubility of permanganate. However, since only two batches of resin (40 L each) are expected to be digested, the total waste generated is limited.
- Research Organization:
- SRS
- Sponsoring Organization:
- DOE
- DOE Contract Number:
- AC09-08SR22470
- OSTI ID:
- 992625
- Report Number(s):
- SRNL-STI-2009-00423
- Country of Publication:
- United States
- Language:
- English
Similar Records
Analysis of Permanganate-Digested Reillex(TM) HPQ Anion Exchange Resin
Permanganate Degradation of Reillex HPQ Ion Exchange Resin for Use in HB-Line
Measurement of Hydrogen Generation Rates during Digestion, Neutralization, Transfer, and Storage of Reillex HPQ Resin
Technical Report
·
Tue Oct 02 00:00:00 EDT 2001
·
OSTI ID:787460
Permanganate Degradation of Reillex HPQ Ion Exchange Resin for Use in HB-Line
Technical Report
·
Wed Jun 02 00:00:00 EDT 1999
·
OSTI ID:7556
Measurement of Hydrogen Generation Rates during Digestion, Neutralization, Transfer, and Storage of Reillex HPQ Resin
Technical Report
·
Tue Oct 02 00:00:00 EDT 2018
·
OSTI ID:1480839