Void Swelling Of Aisi 321 Analog Stainless Steel Irradiated At Low Dpa Rates In The Bn-350 Reactor
Book
·
OSTI ID:966322
In several recently published studies conducted on a Soviet analog of AISI 321 stainless steel irradiated in either fast reactors or light water reactors, it was shown that the void swelling phenomenon extended to temperatures as low as ~300ºC or less, when produced by neutron irradiation at dpa rates in the range 10-7 to 10-8 dpa/sec. Other studies yielded similar results for AISI 316 and the Russian analog of AISI 316. In the current study a blanket duct assembly from BN-350, constructed from the Soviet analog of AISI 321, also exhibits swelling at dpa rates on the order of 10-8 dpa/sec, with voids seen as low as 281oC and only 0.65 dpa. It appears that low-temperature swelling occurs at low dpa rates in 300 series stainless steels in general, and also occurs during irradiations conducted in either fast or mixed spectrum reactors. Therefore it is expected that a similar behavior will be observed in fusion devices as well.
- Research Organization:
- Pacific Northwest National Laboratory (PNNL), Richland, WA (US)
- Sponsoring Organization:
- USDOE
- DOE Contract Number:
- AC05-76RL01830
- OSTI ID:
- 966322
- Report Number(s):
- PNNL-SA-48681; AT6020100
- Country of Publication:
- United States
- Language:
- English
Similar Records
Void Swelling of AISI 321 Analog Stainless Steel Irradiated at Low DPA Rates in the BN-350 Reactor
Characterization of Structural Conditions of AISI 316 Analog Stainless Steel Irradiated in the BN-350 Reactor. In: Fusion Materials Semiannual Progress Report for the period ending December 31, 2003 (DOE/ER-0313/35)
Void Swelling at Low Displacement Rates in Annealed X18H10T Stainless Steel at 4 to 56 DPA and 280-332 degrees centigrade
Journal Article
·
Wed Aug 01 00:00:00 EDT 2007
· Journal of Nuclear Materials, 367-370:990-994
·
OSTI ID:917944
Characterization of Structural Conditions of AISI 316 Analog Stainless Steel Irradiated in the BN-350 Reactor. In: Fusion Materials Semiannual Progress Report for the period ending December 31, 2003 (DOE/ER-0313/35)
Book
·
Tue Aug 24 00:00:00 EDT 2004
·
OSTI ID:15010725
Void Swelling at Low Displacement Rates in Annealed X18H10T Stainless Steel at 4 to 56 DPA and 280-332 degrees centigrade
Book
·
Mon Oct 01 00:00:00 EDT 2001
·
OSTI ID:900225