Rapid self-start of polymer electrolyte fuel cells from sub-freezing temperatures.

Conference ·
OSTI ID:925280

Polymer electrolyte fuel cell (PEFC) systems for light-duty vehicles must be able to start unassisted and rapidly from temperatures below -20 degrees C. Managing buildup of ice within the porous cathode catalyst and electrode structure is the key to self-starting a PEFC stack from subfreezing temperatures. The stack temperature must be raised above the melting point of ice before the ice completely covers the cathode catalyst and shuts down the electrochemical reaction. For rapid and robust self-start it is desirable to operate the stack near the short-circuit conditions. This mode of operation maximizes hydrogen utilization, favors production of waste heat that is absorbed by the stack, and delays complete loss of effective electrochemical surface area by causing a large fraction of the ice to form in the gas diffusion layer rather than in the cathode catalyst layer. Preheating the feed gases, using the power generated to electrically heat the stack, and operating pressures have only small effect on the ability to self-start or the startup time. In subfreezing weather, the stack shut-down protocol should include flowing ambient air through the hot cathode passages to vaporize liquid water remaining in the cathode catalyst. Self-start is faster and more robust if the bipolar plates are made from metal rather than graphite.

Research Organization:
Argonne National Laboratory (ANL)
Sponsoring Organization:
EE
DOE Contract Number:
AC02-06CH11357
OSTI ID:
925280
Report Number(s):
ANL/NE/CP-116067
Country of Publication:
United States
Language:
ENGLISH

Similar Records

Water transport during startup and shutdown of polymer electrolyte fuel cell stacks.
Journal Article · Fri Oct 01 00:00:00 EDT 2010 · J. Power Sources · OSTI ID:984298

Final Report - Subfreezing Start/Stop Protocol for an Advanced Metallic Open Flowfield Fuel Cell Stack
Technical Report · Tue Sep 28 00:00:00 EDT 2010 · OSTI ID:1169585

Cold-start characteristics of polymer electrolyte fuel cells
Conference · Thu Dec 31 23:00:00 EST 2009 · OSTI ID:983923