Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

Role of Intergranular Films in Toughened Ceramics

Conference ·
OSTI ID:7852

Self-reinforced silicon nitride ceramics rely the generation of elongated grains that act as reinforcing elements to gain increases in fracture toughness. However, the size and number of the reinforcing grains must be controlled, along with the matrix grain size, to optimize the fracture toughness and strength. Furthermore, the toughening processes of crack bridging are dependent upon retention of these reinforcing grains during crack extension by an interfacial debonding process. Both the debonding process and the resultant toughening effects are found to be influenced by the composition of the sintering aids which typical are incorporated into the amorphous intergranular films found in these ceramics. Specifically, it is shown that the interface between the intergranular glass and the reinforcing grains is strengthened in the presence of an epitaxial SiAlON layer. In addition, the interface strength increases with the Al and 0 content of the SiAlON layer. Micromechanics modeling indicates that stresses associated with thermal expansion mismatch are a secondary factor in interfacial debonding in these specific systems. On the other hand, first principles atomic cluster calculations reveal that the debonding behavior is consistent with the formation of strong Si-0 and Al-O bonds across the glass-crystalline interface.

Research Organization:
Oak Ridge National Laboratory (ORNL), Oak Ridge, TN
Sponsoring Organization:
USDOE Office of Science
DOE Contract Number:
AC05-96OR22464
OSTI ID:
7852
Report Number(s):
ORNL/CP-102662; KC 02 01 05 0; ON: DE00007852
Country of Publication:
United States
Language:
English

Similar Records

Debonding of interfaces between beta-silicon nitride whiskers and Si-Al-Y oxynitride glasses
Journal Article · Tue Oct 01 00:00:00 EDT 1996 · Acta Materialia · OSTI ID:415389

Microstructural design of silicon nitride with improved fracture toughness. 2: Effects of yttria and alumina additives
Journal Article · Sat Oct 31 23:00:00 EST 1998 · Journal of the American Ceramic Society · OSTI ID:289477

Debonding behavior between [beta]-Si[sub 3]N[sub 4] whiskers and oxynitride glasses with or without an epitaxial [beta]-SiAlON interfacial layer
Journal Article · Fri Jul 09 00:00:00 EDT 1999 · Acta Materialia · OSTI ID:6332048