Superplasticity and joining of zirconia-based ceramics

Conference ·
OSTI ID:750622
Steady-state creep and joining of alumina/zirconia composites containing alumina volume fractions of 20, 60, and 85% have been investigated between 1,250 and 1,350 C. Superplasticity of these compounds is controlled by grain-boundary sliding and the creep rate is a function of alumina volume fraction, not grain size. Using the principles of superplasticity, pieces of the composite have been joined by applying the stress required to achieve 5 to 10% strain to form a strong interface at temperatures as low as 1,200 C.
Research Organization:
Argonne National Lab., IL (US)
Sponsoring Organization:
US Department of Energy (US)
DOE Contract Number:
W-31109-ENG-38
OSTI ID:
750622
Report Number(s):
ANL/ET/CP-100681
Country of Publication:
United States
Language:
English

Similar Records

Superplasticity and joining of zirconia-based ceramics
Conference · Sat Jul 01 00:00:00 EDT 2000 · OSTI ID:20104663

Current understanding of superplastic deformation of Y-TZP and its application to joining.
Journal Article · Sun Apr 15 00:00:00 EDT 2001 · Mater. Sci. Eng. A · OSTI ID:942821

Joining of yttria-tetragonal stabilized zirconia polycrystals using nanocrystals
Journal Article · Fri Aug 06 00:00:00 EDT 1999 · Scripta Materialia · OSTI ID:691328