Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

Boron-filled elastomers (SANL 252-056). [Vinyl copolymer; Viton A fluoroelastomer; physical characteristics]

Technical Report ·
DOI:https://doi.org/10.2172/7363488· OSTI ID:7363488
A series of boron-filled vinyl copolymer elastomer (VCE) and Viton A fluoroelastomer formulations was prepared and the physical characteristics of the cured formulations determined. Their weight loss on heating to 300/sup 0/C, as determined by two different analytical methods, did not agree. The presence of up to 0.23 percent boric acid in the boron powders used to fill a standard boron-filled VCE elastomer did not appear to affect the physical characteristics of the cured formulation. 7 tables. (auth)
Research Organization:
Mound Lab., Miamisburg, Ohio (USA)
DOE Contract Number:
E(33-1)-GEN-53
OSTI ID:
7363488
Report Number(s):
MLM-2315
Country of Publication:
United States
Language:
English