Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

Use of nickel hydroxide in pressed plate electrodes

Patent ·
OSTI ID:7328886
The addition of 0.1 to 5 percent Ni(OH)/sub 2/ to the anode material of an alkaline battery helps maintain the rechargeability of the anode for many cycles. Typical anode material consists of up to /sup 1///sub 3/ Cd particles 5 to 10 ..mu..m in diameter, with the remainder almost entirely CdO. About 1 percent Ni(OH)/sub 2/ and 1 percent Teflon are added. Charge retention capacity is improved about 25 percent with the addition of nickel hydroxide. (RWR)
Assignee:
General Electric Co.
Patent Number(s):
US 3870562
OSTI ID:
7328886
Country of Publication:
United States
Language:
English