Charpy impact test results of ferritic alloys from the HFIR(High Flux Isotope Reactor)-MFE-RB2 test

Technical Report ·
OSTI ID:6566423
Miniature Charpy specimens of HT-9 in base metal, weld metal and heat affected zone (HAZ) metal conditions, and 9Cr-1Mo in base metal and weld metal conditions have been tested following irradiation in HFIR-MFE-RB2 at 55/sup 0/C to approx. =10 dpa. All specimen conditions have degraded properties (both DBTT and USE) in comparison with specimens irradiated to lower dose. 9Cr-Mo degraded more than HT-9 and weld metal performed worse than base metal which performed worse than HAZ material. Property degradation was approximately linear as a function of dose, indicating that degradation response had not saturated by 10 dpa.
Research Organization:
Hanford Engineering Development Lab., Richland, WA (USA)
DOE Contract Number:
AC06-76FF02170
OSTI ID:
6566423
Report Number(s):
HEDL-7655; ON: DE87009521
Country of Publication:
United States
Language:
English