Quantitative methods in fractography; Proceedings of the Symposium on Evaluation and Techniques in Fractography, Atlanta, GA, Nov. 10, 1988
Papers are presented on the application of quantitative fractography and computed tomography to fracture processes in materials, the relationships between fractographic features and material toughness, the quantitative analysis of fracture surfaces using fractals, and the analysis and interpretation of aircraft component defects by means of quantitative fractography. Also discussed are the characteristics of hydrogen-assisted cracking measured by the holding-load and fractographic method, a fractographic study of isolated cleavage regions in nuclear pressure vessel steels and their weld metals, a fractographic and metallographic study of the initiation of brittle fracture in weldments, cracking mechanisms for mean stress/strain low-cycle multiaxial fatigue loadings, and corrosion fatigue crack arrest in Al alloys.
- OSTI ID:
- 6459209
- Report Number(s):
- CONF-8811253-
- Resource Relation:
- Conference: ASTM symposium on evaluation and techniques in fractography, Atlanta, GA (USA), 10 Nov 1988; Related Information: ASTM Special Technical Publication, No. 1085
- Country of Publication:
- United States
- Language:
- English
Similar Records
SEM stereo-section fractography observations. Final report
Fractography of modern engineering materials: composites and metals
Related Subjects
FRACTOGRAPHY
MEETINGS
AIRCRAFT COMPONENTS
COMPUTERIZED TOMOGRAPHY
CRACK PROPAGATION
CRACKS
FRACTALS
FRACTURE PROPERTIES
HYDROGEN EMBRITTLEMENT
LEADING ABSTRACT
MATERIALS
METALLOGRAPHY
METALS
PRESSURE VESSELS
WELDED JOINTS
ABSTRACTS
CONTAINERS
DIAGNOSTIC TECHNIQUES
DOCUMENT TYPES
ELEMENTS
EMBRITTLEMENT
JOINTS
MECHANICAL PROPERTIES
TOMOGRAPHY
360000* - Materials