Electrical properties in the system (La/sub 1-x/Ca/sub x/)CoO/sub 3/ (0. 1 less than or equal to x less than or equal to 0. 5)

Journal Article · · J. Solid State Chem.; (United States)
 [1]; ;
  1. Osaka Prefectural Industrial Research Inst., Japan
The electrical resistivity of (La/sub 1-x/Ca/sub x/)CoO/sub 3/(0.1 less than or equal to X less than or equal to0.5) was measured in the temperature range from 80 to 300K. Cobaltite with x less than or equal to 0.15 is a semiconductor, but the specimen with chemical composition 0.2 less than or equal to x less than or equal to 0.5 is metallic. The change of temperature dependence of electrical resistivity has a break point around T/sub c/. The value of the logarithm of the specific electrical resistivity (log p) at 300K has a minimum at x = 0.4, and this result is explained by the Zener double-exchange mechanism.
OSTI ID:
6432196
Journal Information:
J. Solid State Chem.; (United States), Journal Name: J. Solid State Chem.; (United States) Vol. 44:2; ISSN JSSCB
Country of Publication:
United States
Language:
English