Fractography of ceramic and metal failures
Book
·
OSTI ID:6097709
STP 827 is organized into the two broad areas of ceramics and metals. The ceramics section covers fracture analysis techniques, surface analysis techniques, and applied fractography. The metals section covers failure analysis techniques, and latest approaches to fractography, and applied fractography.