Subcritical crack growth in Y-TZP and Al[sub 2]O[sub 3]-toughened Y-TZP

Journal Article · · Journal of the American Ceramic Society; (United States)
; ; ;  [1]
  1. Technical Univ. of Hamburg-Harburg (Germany). Advanced Ceramics Group
Crack velocity curves for Y-TZP and Al[sub 2]O[sub 3]-toughened Y-TZP were determined for long cracks in compact tension specimens with an in situ fracture device on the stage of an optical microscope. Indications for a crack velocity threshold were found for both materials. It is recognized that the dependence of the shielding term on the crack-tip stress field renders transformation-toughened materials particularly susceptible to stress-corrosion cracking. This interrelation leads to the definition of a steady-state velocity at constant applied stress intensity factor. This velocity is obtained in the situation where the shielding term is fully defined by the present crack-tip stress field, not depending on prior loading history.
OSTI ID:
5726525
Journal Information:
Journal of the American Ceramic Society; (United States), Journal Name: Journal of the American Ceramic Society; (United States) Vol. 76:10; ISSN 0002-7820; ISSN JACTAW
Country of Publication:
United States
Language:
English

Similar Records

Crack shielding in Ce-TZP/Al{sub 2}O{sub 3} composites: Comparison of fatigue and sustained crack growth specimens
Journal Article · Fri Dec 31 23:00:00 EST 1993 · Journal of the American Ceramic Society · OSTI ID:142240

Transient subcritical crack-growth behavior in transformation-toughened ceramics
Journal Article · Sun Dec 31 23:00:00 EST 1989 · Acta Metallurgica et Materialia; (United States) · OSTI ID:7018582

The closure of indentation cracks and strength recovery by low temperature ageing in Y-TZP
Journal Article · Thu Oct 01 00:00:00 EDT 1992 · Scripta Metallurgica et Materialia; (United States) · OSTI ID:7018711