Gas tungsten arc welding of aluminum alloys 6XXX. Welding procedure specification. Supplement 1. Records of procedure qualification tests. [6061 and 6063]

Technical Report ·
OSTI ID:5636327

Procedure WPS-1003 is qualified under Section IX of the ASME Boiler and Pressure Vessel Code for gas tungsten arc welding of aluminum alloys 6061 and 6063 (P-23), in thickness range 0.035 to 0.516 inch; filler metal is ER4043 (F-23) or ER5356 (F-22); shielding gas is argon.