Particle characterization. Quarterly report October--December, 1970

Technical Report ·
DOI:https://doi.org/10.2172/555393· OSTI ID:555393

In the manufacture of Extex (XTX 8003, 80% PETN, 20% Sylgard silicone rubber), the formulation is mixed for about five hours. Freon MF is added in the proportions of fur pounds Extex to one quart Freon, to enhance the mixing at lower power than would otherwise be the case. After mixing, the formulation is milled on a three-roll rubber mill for a total of 25 passes. The study of the effects of roll milling on Extex was started; the visual results are indicative that a considerable reduction in crystal size occurs during the formulation process.

Research Organization:
Mason and Hanger-Silas Mason Co., Inc., Amarillo, TX (United States)
Sponsoring Organization:
USDOE, Washington, DC (United States)
DOE Contract Number:
AC04-91AL65030
OSTI ID:
555393
Report Number(s):
MHSMP--70-50; PX--70-50; ON: DE97009039
Country of Publication:
United States
Language:
English

Similar Records

HE formulation. Quarterly report, October--December, 1971
Technical Report · Thu Dec 30 23:00:00 EST 1971 · OSTI ID:532465

He formulation. Quarterly report, April--June 1965
Technical Report · Thu Dec 30 23:00:00 EST 1965 · OSTI ID:522537

Extrudable explosives. Quarterly report, October--December, 1971
Technical Report · Sat Dec 30 23:00:00 EST 1972 · OSTI ID:537251