Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

Characterization of polymers for microcellular foams

Technical Report ·
OSTI ID:5398476
We have measured, by {sup 1}H and {sup 13}C nuclear magnetic resonance (NMR), the percent deuteration, the tacticity and the purity of several polymers and one solvent used in the preparation of microcellular foams. The percent deuteration was measured for polystyrene, polyacrylonitrile and polyethylene. The tacticities of polystyrene and polyacrylonitrile were determined. The purity and degradation products of polyacrylonitrile and maleic anhydride were examined. This report documents the experimental procedures and results of these measurements.
Research Organization:
Sandia National Labs., Albuquerque, NM (United States)
Sponsoring Organization:
DOE; USDOE, Washington, DC (United States)
DOE Contract Number:
AC04-76DP00789
OSTI ID:
5398476
Report Number(s):
SAND-91-1591; ON: DE92012444
Country of Publication:
United States
Language:
English