Gas tungsten arc welding of aluminum alloys 1XXX and 3003 to 3004, 5052 and 5X54. Welding procedure specification
Technical Report
·
OSTI ID:5139164
Procedure WPS-2201 is qualified under Section IX of the ASME Boiler and Pressure Vessel for gas tungsten arc welding of aluminum alloys 1060, 1100, and 3003 (P-21) to 3004, 5052, 5154, and 5454 (P-22), in thickness range 0.062 to 0.5 in.; filler metal is ER5356 (F-22); shielding gas is argon.
- Research Organization:
- Oak Ridge National Lab., TN (USA)
- DOE Contract Number:
- AC05-84OR21400
- OSTI ID:
- 5139164
- Report Number(s):
- ORNL/M-37; ON: DE86001523
- Country of Publication:
- United States
- Language:
- English
Similar Records
Welding procedure specification. Suppliment 1. Records of procedure qualification tests. Gas tungsten arc welding of aluminum alloys 1XXX and 3003 to 3004, 5052 and 5X54. [1060, 1100, and 3003 to 3004, 5052, 5154, and 5454]
Gas tungsten arc welding of aluminum alloys 3004, 5052, and 5X54. Welding procedure specification
Welding procedure specification. Supplement 1. Records of procedure qualification tests. Gas tungsten arc welding of aluminum alloys 3004, 5052, and 5X54
Technical Report
·
Sun Jun 01 00:00:00 EDT 1986
·
OSTI ID:5139164
Gas tungsten arc welding of aluminum alloys 3004, 5052, and 5X54. Welding procedure specification
Technical Report
·
Thu Aug 01 00:00:00 EDT 1985
·
OSTI ID:5139164
Welding procedure specification. Supplement 1. Records of procedure qualification tests. Gas tungsten arc welding of aluminum alloys 3004, 5052, and 5X54
Technical Report
·
Sun Jun 01 00:00:00 EDT 1986
·
OSTI ID:5139164