Localized corrosion and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Annual progress report, June 1, 1977--March 31, 1978
Localized corrosion (pitting) experiments have been performed on single-phase austenitic 304 stainless steels and on duplex 304 steels containing 6 to 8% retained delta ferrite as a result of rapid solidification (welding). Experimental variables included thermomechanical treatment, solution pH, chloride concentration and solution temperature.
- Research Organization:
- Rensselaer Polytechnic Inst., Troy, N.Y. (USA). Dept. of Materials Engineering
- DOE Contract Number:
- EY-76-S-02-2462
- OSTI ID:
- 5004358
- Report Number(s):
- COO-2462-4
- Country of Publication:
- United States
- Language:
- English
Similar Records
Localized corrosion and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Annual progress report, June 1, 1978--March 31, 1979
Localized corrosion and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Annual progress report, June 1, 1979-March 31, 1980
Pitting and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Technical progress report No. 2, June 1, 1975--May 31, 1976
Technical Report
·
Thu Mar 01 00:00:00 EST 1979
·
OSTI ID:5004358
Localized corrosion and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Annual progress report, June 1, 1979-March 31, 1980
Technical Report
·
Sat Mar 01 00:00:00 EST 1980
·
OSTI ID:5004358
Pitting and stress corrosion cracking behavior of austenitic stainless steel weldments containing retained ferrite. Technical progress report No. 2, June 1, 1975--May 31, 1976
Technical Report
·
Thu Jan 01 00:00:00 EST 1976
·
OSTI ID:5004358
Related Subjects
36 MATERIALS SCIENCE
STAINLESS STEEL-304
PITTING CORROSION
AUSTENITIC STEELS
PH VALUE
TEMPERATURE DEPENDENCE
ALLOYS
CHEMICAL REACTIONS
CHROMIUM ALLOYS
CHROMIUM STEELS
CHROMIUM-NICKEL STEELS
CORROSION
CORROSION RESISTANT ALLOYS
HEAT RESISTING ALLOYS
IRON ALLOYS
IRON BASE ALLOYS
NICKEL ALLOYS
STAINLESS STEELS
STEELS
360105* - Metals & Alloys- Corrosion & Erosion
STAINLESS STEEL-304
PITTING CORROSION
AUSTENITIC STEELS
PH VALUE
TEMPERATURE DEPENDENCE
ALLOYS
CHEMICAL REACTIONS
CHROMIUM ALLOYS
CHROMIUM STEELS
CHROMIUM-NICKEL STEELS
CORROSION
CORROSION RESISTANT ALLOYS
HEAT RESISTING ALLOYS
IRON ALLOYS
IRON BASE ALLOYS
NICKEL ALLOYS
STAINLESS STEELS
STEELS
360105* - Metals & Alloys- Corrosion & Erosion