Metal matrix composite of an iron aluminide and ceramic particles and method thereof

Patent ·
OSTI ID:489099

A metal matrix composite comprising an iron aluminide binder phase and a ceramic particulate phase such as titanium diboride, zirconium diboride, titanium carbide and tungsten carbide is made by heating a mixture of iron aluminide powder and particulates of one of the ceramics such as titanium diboride, zirconium diboride, titanium carbide and tungsten carbide in a alumina crucible at about 1,450 C for about 15 minutes in an evacuated furnace and cooling the mixture to room temperature. The ceramic particulates comprise greater than 40 volume percent to about 99 volume percent of the metal matrix composite.

Research Organization:
Lockheed Martin Energy Syst Inc
Sponsoring Organization:
USDOE, Washington, DC (United States)
DOE Contract Number:
AC05-84OR21400
Assignee:
Lockheed Martin Energy Systems, Inc., Oak Ridge, TN (United States)
Patent Number(s):
US 5,637,816/A/
Application Number:
PAN: 8-517,638
OSTI ID:
489099
Country of Publication:
United States
Language:
English

Similar Records

Metal matrix composite of an iron aluminide and ceramic particles and method thereof
Patent · Tue Dec 31 23:00:00 EST 1996 · OSTI ID:870994

Mechanical properties of near-{gamma} titanium aluminides reinforced with high volume percentages of TiB{sub 2}
Journal Article · Mon Apr 15 00:00:00 EDT 1996 · Scripta Materialia · OSTI ID:230761

Process for the fabrication of ceramic fiber reinforced titanium aluminide
Conference · Thu Oct 01 00:00:00 EDT 1992 · Ceramic Engineering and Science Proceedings; (United States) · OSTI ID:7110544