Creep of zirconium in water from 400 degree to 600 degree F
Technical Report
·
OSTI ID:481274
2000-hour creep tests were made on 0.015-inch zirconium wire in water at temperatures ranging from 400 deg to 600 deg F. Values of secondary creep were determined and limiting creep stresses were obtained for creep rates of 0.1% and 1.0% in 1000 hours. Total elongation was measured after the test run of 2000 hours.
- Research Organization:
- Sylvania Electric Products, Inc., Bayside, NY (United States)
- OSTI ID:
- 481274
- Report Number(s):
- AD-A--321741/1/XAB; SEP--54; CNN: Contract AT-30-1-GEN-366
- Country of Publication:
- United States
- Language:
- English
Similar Records
THE CREEP BEHAVIOUR OF THE MAGNESIUM-ZIRCONIUM ALLOY ZA AT 400 AND 450 C IN CARBON DIOXIDE CONTAINING /approximately equals/200 PPM MOISTURE
CREEP OF ZIRCONIUM
Tensile properties of zirconium at elevated temperatures
Journal Article
·
Thu Feb 28 23:00:00 EST 1963
· Journal of Nuclear Materials (Netherlands)
·
OSTI ID:4687408
CREEP OF ZIRCONIUM
Journal Article
·
Thu May 01 00:00:00 EDT 1958
· Nippon Kinzoku Gakkaishi (Japan)
·
OSTI ID:4268334
Tensile properties of zirconium at elevated temperatures
Technical Report
·
Mon Apr 03 23:00:00 EST 1950
·
OSTI ID:195063