DISPERSION STRENGTHENED NICKEL-BASE ALLOYS. Progress Report No. 1, March 1 to April 30, 1963
Technical Report
·
OSTI ID:4721219
Dispersion strengthened Ni-base alloys (80% Ni--20% Cr) were prepared by the mechanical mixing of Nichrome and thorium oxide powders. The compositions and principal fabrication variables of 5 extruded alloys are tabulated. (P.C.H.)
- Research Organization:
- New England Materials Lab., Inc., Medford, Mass.
- NSA Number:
- NSA-17-023959
- OSTI ID:
- 4721219
- Report Number(s):
- NP-12793
- Country of Publication:
- United States
- Language:
- English
Similar Records
DISPERSION STRENGTHENED NICKEL-BASE ALLOYS. Progress Report No. 2, May 1 to June 30, 1963
DISPERSION-STRENGTHENED NICKEL-BASE ALLOYS. Progress Report No. 3, July 1 to August 30, 1963
DISPERSION STRENGTHENED NICKEL-BASE ALLOYS. Final Report, March 1- December 31, 1963
Technical Report
·
Thu Aug 01 00:00:00 EDT 1963
·
OSTI ID:4654831
DISPERSION-STRENGTHENED NICKEL-BASE ALLOYS. Progress Report No. 3, July 1 to August 30, 1963
Technical Report
·
Thu Oct 17 00:00:00 EDT 1963
·
OSTI ID:4171126
DISPERSION STRENGTHENED NICKEL-BASE ALLOYS. Final Report, March 1- December 31, 1963
Technical Report
·
Sun Feb 23 23:00:00 EST 1964
·
OSTI ID:4034243