POWDER METALLURGY FOR SUPERALLOYS AND REFRACTORY METALS
Journal Article
·
· Progr. Powder Met.
OSTI ID:4678295
- Research Organization:
- New England Materials Lab., Inc., Medford, Mass.
- NSA Number:
- NSA-19-002774
- OSTI ID:
- 4678295
- Journal Information:
- Progr. Powder Met., Vol. Vol: 20; Other Information: Orig. Receipt Date: 31-DEC-65
- Country of Publication:
- Country unknown/Code not available
- Language:
- English
Similar Records
VAPO-METALLURGY. ARTICLE III. PREPARATION OF REFRACTORY METAL POWDERS WITH UNUSUAL PROPERTIES
POWDER METALLURGY OF REFRACTORY METALS
Powder metallurgy of heat-resistant alloys and refractory metals; Poroshkovaya metallurgiya zharoprochnykh splavov i tugoplavkikh metallov
Journal Article
·
Tue Jun 01 00:00:00 EDT 1965
· J. Metals
·
OSTI ID:4678295
POWDER METALLURGY OF REFRACTORY METALS
Journal Article
·
Mon Sep 01 00:00:00 EDT 1958
· Metal Progr.
·
OSTI ID:4678295
Powder metallurgy of heat-resistant alloys and refractory metals; Poroshkovaya metallurgiya zharoprochnykh splavov i tugoplavkikh metallov
Book
·
Tue Jan 01 00:00:00 EST 1974
·
OSTI ID:4678295
+1 more