Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

Metallurgical examination of gun barrel screws

Technical Report ·
DOI:https://doi.org/10.2172/446024· OSTI ID:446024

The examination was conducted to determine the extent of degradation that had occurred after a series of firings; these screws prevent live rounds of ammunition from being loaded into the firing chamber. One concern is that if the screw tip fails and a live round is accidentally loaded into the chamber, a live round could be fired. Another concern is that if the blunt end of the screw begins to degrade by cracking, pieces could become small projectiles during firing. All screws used in firing 100 rounds or more exhibited some degree degradation, which progressively worsened as the number of rounds fired increased. (SEM, metallography, x-ray analysis, and microhardness were used.) Presence of cracks in these screws after 100 fired rounds is a serious concern that warrants the discontinued use of these screws. The screw could be improved by selecting an alloy more resistant to thermal and chemical degradation.

Research Organization:
Oak Ridge Y-12 Plant, TN (United States)
Sponsoring Organization:
USDOE, Washington, DC (United States)
DOE Contract Number:
AC05-96OR22464
OSTI ID:
446024
Report Number(s):
Y/DV--1401; ON: DE97002739
Country of Publication:
United States
Language:
English

Similar Records

Physical and chemical interactions at the bore surface of a Ta-10W gun barrel liner
Book · Sat Jun 01 00:00:00 EDT 1996 · OSTI ID:237695

Elastic interaction of a wedge crack with a screw dislocation
Journal Article · Thu Mar 14 23:00:00 EST 1985 · J. Appl. Phys.; (United States) · OSTI ID:5989590

Firearm equipped with live round inhibiting means and method of making same