A METHOD FOR ROLLING URANIUM FOIL

Technical Report ·
OSTI ID:4355825
Uranium-buttons may be rolled in a simple process by breaking and firing, plating, annealing at 600 deg C for 1/2 hr in a low pressure vacuum furnace, rolling immediately while still hot and then annealing. If cross rolling is done, the piece can be given two passes 90 deg to each other at the same reduction without being annealed between passes. If a 10 to 20% reduction is wanted on every 90 deg turn, the piece should be annealed between each pass. Four passes at 5% with 200 deg heat treatmert between each pass is not as good as one 20% reduction pass. (F.S.)
Research Organization:
Los Alamos Scientific Lab., N. Mex.
NSA Number:
NSA-12-000913
OSTI ID:
4355825
Report Number(s):
LAMS-626
Country of Publication:
Country unknown/Code not available
Language:
English

Similar Records

METHOD OF ROLLING URANIUM
Patent · Sat Aug 01 00:00:00 EDT 1959 · OSTI ID:4206172

On the Rolling of Uranium Rods by Grooved Rolls
Journal Article · Wed Dec 31 23:00:00 EST 1958 · Nippon Genshiryoku Gakkai-Shi · OSTI ID:4206202

ROLLING OF URANIUM
Technical Report · Thu Jan 31 23:00:00 EST 1957 · OSTI ID:4341875