SUMMARY OF SPECIMEN CORROSION DATA FROM SLURRY BLANKET MOCK-UP RUN SM-3
Examination of corrosion specimens from the 948 hour slurry blanket mock- up Run SM-3 lndicated generally low attack rates on type 347 stainless steel, titanium -75A, and Zircaloy-2. The upstream coupon of the array, of type 347 stainless steel, suffered moderate but more severe attack. Coupons of SA-212 grade B carbon steel were severely attacked. No stress corrosion cracking was noted on samples, placed in the pressurizer, of types 347 and AM 350 stainless steels, titanium aluminum--vanadium alloy, or Zircaloy-2. (auth)
- Research Organization:
- Oak Ridge National Lab., Tenn.
- DOE Contract Number:
- W-7405-ENG-26
- NSA Number:
- NSA-12-001368
- OSTI ID:
- 4328381
- Report Number(s):
- CF-57-10-5
- Country of Publication:
- United States
- Language:
- English
Similar Records
EXAMINATION OF CORROSION SPECIMENS FROM SLURRY BLANKET MOCKUP RUN SM-4
EXAMINATION OF CORROSION SPECIMENS FROM SLURRY BLANKET MOCKUP RUNS SM-6 THROUGH SM-9
EXAMINATION OF CORROSION SPECIMENS FROM SLURRY BLANKET MOCKUP RUN SM-5
Technical Report
·
Sun Jun 01 00:00:00 EDT 1958
·
OSTI ID:4303599
EXAMINATION OF CORROSION SPECIMENS FROM SLURRY BLANKET MOCKUP RUNS SM-6 THROUGH SM-9
Technical Report
·
Thu May 26 00:00:00 EDT 1960
·
OSTI ID:4176770
EXAMINATION OF CORROSION SPECIMENS FROM SLURRY BLANKET MOCKUP RUN SM-5
Technical Report
·
Thu Aug 28 00:00:00 EDT 1958
·
OSTI ID:4296106