Effect of temperature and strain rate on the tensile properties of aluminum- -boron, epoxy--boron, and epoxy--graphite composites. Final report
The effects of strain rates from 0.00008 to 0.4/sec on tensile strengths and moduli of 6061 aluminum-46.5 vol% boron at temperatures up to 1000 deg F, of unidirectional and cross-ply epoxy-50 vol% boron composites at temperatures up to 500 deg F and of crossply epoxy --80 vol% graphite composites at temperatures up to 250 deg F were measured. Longitudinal properties were reduced moderately at high temperatures and were only slightly higher at high strain rates than at low strain rates. Transverse properties decreased rapidly with temperature and were either unaffected by high strain rates, particularly at low temperatures, or were substantially increased, especially at high temperatures, in both aluminum- and epoxy-based systems. (auth)
- Research Organization:
- Naval Research Lab., Washington, D.C. (USA)
- NSA Number:
- NSA-29-027191
- OSTI ID:
- 4326897
- Report Number(s):
- AD-763656; NRL-MR-2609
- Resource Relation:
- Other Information: Orig. Receipt Date: 30-JUN-74
- Country of Publication:
- United States
- Language:
- English
Similar Records
Validation of reduced composite allowable variation via prestressing. Final report July 1973--June 1974. [Boron/epoxy prepreg tape: rigidit 5505/4 C/B, W/. gamma. B]
Machining characteristics of graphite/epoxy composite. Ph.D. Thesis
Related Subjects
Ceramics
& Other Materials-Ceramics & Cermets-Properties
Structure & Phase Studies
*ALUMINIUM ALLOYS- TENSILE PROPERTIES
*BORON ALLOYS- TENSILE PROPERTIES
*COMPOSITE MATERIALS- TENSILE PROPERTIES
*EPOXIDES- TENSILE PROPERTIES
*GRAPHITE- TENSILE PROPERTIES
STRAINS
TEMPERATURE DEPENDENCE