IMPROVEMENTS IN OR RELATING TO HEAT TREATMENT OF URANIUM
Patent
·
OSTI ID:4262897
A heat treatment for U is proposed which reduces grain size of castings. It consists of heating in a salt bath to 735 C for 13 min followed by a quench in CaCl/sub 2/ brine at -30 C. Average grain size of macro 0.25 mm is obtained. (T.R.H.)
- Research Organization:
- Originating Research Org. not identified
- NSA Number:
- NSA-13-011930
- OSTI ID:
- 4262897
- Report Number(s):
- GB 812123
- Resource Relation:
- Other Information: Orig. Receipt Date: 31-DEC-59
- Country of Publication:
- United Kingdom
- Language:
- English
Similar Records
SUMMARY OF PROGRESS ON THE STUDY OF BETA TREATMENT OF URANIUM, SEPTEMBER 1 TO NOVEMBER 30, 1960
GRAIN REFINEMENT OF CAST URANIUM BY HEAT TREATMENT
IMPROVEMENTS IN FISSIONABLE MATERIALS FOR USE IN NUCLEAR REACTORS AND IN THE METHODS OF MANUFACTURING SUCH MATERIALS
Technical Report
·
Tue Dec 27 00:00:00 EST 1960
·
OSTI ID:4262897
GRAIN REFINEMENT OF CAST URANIUM BY HEAT TREATMENT
Technical Report
·
Mon Jul 01 00:00:00 EDT 1957
·
OSTI ID:4262897
IMPROVEMENTS IN FISSIONABLE MATERIALS FOR USE IN NUCLEAR REACTORS AND IN THE METHODS OF MANUFACTURING SUCH MATERIALS
Patent
·
Wed Oct 14 00:00:00 EDT 1959
·
OSTI ID:4262897