Grain growth in dispersion strengthened superalloys by moving zone heat treatments
Journal Article
·
· Metall. Trans., v. 6, no. 1, pp. 179-188
- Research Organization:
- International Nickel Co. Inc., Suffern, NY
- Sponsoring Organization:
- USDOE
- NSA Number:
- NSA-31-017472
- OSTI ID:
- 4238466
- Journal Information:
- Metall. Trans., v. 6, no. 1, pp. 179-188, Other Information: Orig. Receipt Date: 30-JUN-75
- Country of Publication:
- Country unknown/Code not available
- Language:
- English
Similar Records
Effect of primary grain size on the secondary recrystallization of mechanically alloyed oxide dispersion strengthened Ni-base superalloy
On the influence of grain morphology on creep deformation and damage mechanisms in directionally solidified and oxide dispersion strengthened superalloys
The formation of precipitate free zones and the growth of grain boundary carbides in the nickel-base superalloy NIMONIC PE16
Journal Article
·
Thu Feb 01 00:00:00 EST 1996
· Metallurgical Transactions, A
·
OSTI ID:4238466
+3 more
On the influence of grain morphology on creep deformation and damage mechanisms in directionally solidified and oxide dispersion strengthened superalloys
Journal Article
·
Mon Apr 01 00:00:00 EST 1996
· Metallurgical Transactions, A
·
OSTI ID:4238466
The formation of precipitate free zones and the growth of grain boundary carbides in the nickel-base superalloy NIMONIC PE16
Journal Article
·
Wed Jan 01 00:00:00 EST 1997
· Acta Materialia
·
OSTI ID:4238466
Related Subjects
N50230* -Metals
Ceramics
& Other Materials-Metals & Alloys-Properties
Structure & Phase Studies
*INCONEL ALLOYS- GRAIN GROWTH
*NICKEL BASE ALLOYS- GRAIN GROWTH
*YTTRIUM OXIDES- GRAIN GROWTH
ALUMINIUM ALLOYS
CHROMIUM ALLOYS
HEAT TREATMENTS
MOLYBDENUM ALLOYS
TANTALUM ALLOYS
TITANIUM ALLOYS
TUNGSTEN ALLOYS
Ceramics
& Other Materials-Metals & Alloys-Properties
Structure & Phase Studies
*INCONEL ALLOYS- GRAIN GROWTH
*NICKEL BASE ALLOYS- GRAIN GROWTH
*YTTRIUM OXIDES- GRAIN GROWTH
ALUMINIUM ALLOYS
CHROMIUM ALLOYS
HEAT TREATMENTS
MOLYBDENUM ALLOYS
TANTALUM ALLOYS
TITANIUM ALLOYS
TUNGSTEN ALLOYS