ADDITIONAL TESTS ON THE CORROSION OF CARBON STEEL FOLLOWING THE TURCO-4512 DECONTAMINATION PROCESS
Technical Report
·
OSTI ID:4180757
Carbon steel, 304 stainless steel, and Zircaloy-2 coupons were treated in Turco-4512-2b inhibited phosphoric acid decontaminating solution and then charged in a pH 10, 290 deg C recirculating water loop. The decontaminating solution pretreatment did not affect the corrosion behavior of 304 s/s or Zircaloy-2 but did increase the carbon steel initial penetrations by a factor of 2 and the corrosion product film weights by a factor of 1.7 over those of the nontreated carbon steel coupons. The corrosion rate of the carbon steel coupons was not increased by the decontaminating solution pretreatment. (auth)
- Research Organization:
- General Electric Co. Hanford Atomic Products Operation, Richland, Wash.
- DOE Contract Number:
- W-31-109-ENG-52
- NSA Number:
- NSA-14-016961
- OSTI ID:
- 4180757
- Report Number(s):
- HW-62690
- Country of Publication:
- United States
- Language:
- English
Similar Records
DECONTAMINATION STUDIES FOR HAPO HIGH TEMPERATURE REACTOR RECIRCULATION SYSTEMS. Progress Report, June 1958-June 1959
Evaluation of N-Reactor piping decontamination procedure for effectiveness and materials corrosion
CORROSION OF ZR-2 AND 304 STAINLESS STEEL FOLLOWING THE TURCO-4501 DECONTAMINATION PROCESS
Technical Report
·
Wed Jun 10 00:00:00 EDT 1959
·
OSTI ID:4207485
Evaluation of N-Reactor piping decontamination procedure for effectiveness and materials corrosion
Technical Report
·
Tue Aug 01 00:00:00 EDT 1967
·
OSTI ID:10120753
CORROSION OF ZR-2 AND 304 STAINLESS STEEL FOLLOWING THE TURCO-4501 DECONTAMINATION PROCESS
Technical Report
·
Sun Apr 19 23:00:00 EST 1959
·
OSTI ID:4205242