Skip to main content
U.S. Department of Energy
Office of Scientific and Technical Information

IMPROVEMENTS IN IRRADIATION PROCESS

Patent ·
OSTI ID:4174511
BS>The preparation of stable, cross-linked polypropylene by irradiation is described. In an example, sections of polypropylene were irradiated to 40 x 10/sup 6/ rep in N/sub 2/ over the range 60 to 200 deg C and percent cross- linking was determined by dissolution in toluene. It was found that maximum cross-linking occurs at 100 to 125 deg C. In other examples it is shown that annealing between 130 and 200 deg C results in a flexible product. The polypropylene can be blended with polyethylene prior to irradiation to produce another series of useful products. (T.R.H.)
Research Organization:
Originating Research Org. not identified
NSA Number:
NSA-14-011658
OSTI ID:
4174511
Report Number(s):
GB 831914
Country of Publication:
United Kingdom
Language:
English

Similar Records

POLYETHYLENE OF IMPROVED STABILITY
Patent · Wed Aug 26 00:00:00 EDT 1959 · OSTI ID:4168933

STABLE IRRADIATED POLYETHYLENE
Patent · Tue Mar 22 23:00:00 EST 1960 · OSTI ID:4174732

IMPROVEMENTS IN IRRADIATED OLEFIN POLYMERS
Patent · Thu Mar 31 23:00:00 EST 1960 · OSTI ID:4146967